The first step takes about 2 days. During the Cryo process, a transformation in the metal takes place that transforms soft carbon (retained austenite) into smaller and stronger carbon (martensite). After the cryogenic step, most metal objects are then subjected to a specific heating and cooling sequence to allow metal to stabilize it's new chemical composition. Our system is a dry process, your object never is submersed in liquid Nitrogen. After the Cryopro TM Process is completed, the material is less brittle, stronger and much more durable than before.
Field Test Results | |||
|---|---|---|---|
| Tool Type | Company | Tool Material | Results |
| Sewing Needle | Pant Mfg | Steel | 6000% |
| Insert | Engine Rebuilder | CBN (Diamond) | 400% |
| Broach | Auto Mfg. | Hi Nickel | 250% |
| Broach | Metal Milling Co. | Carbide | 300% |
| Chipper | Box Mfg. | Carbide | 500% |
| Deburring | University Study | Inconol | 400% |
| Dentistry | Dentist | 400 Stainless | 500% |
| Die | Casting Company | Hi Ni Alloy | 300% |
| Drills | Aircraft Mfg | M42,M7,C2 | 300% |
| Electrode | 7 Studies | Welding | 600% |
| End Mill | Aerospace Mfg | M42 | 450% |
| Face Mill | Aerospace | C2 Carbide | 400% |
| Gear Cutter | Major Mfg. | Ti-N Coated | 350% |
| Hob | Turbine Mfg. | M2, M7 | 300% |
| Key Cutter | Aircraft Mfg. | M2, M7 | 250% |
| Milling | Aircraft Mfg. | M7 | 250% |
| Punching | Major Mfg. | M7 | 600% |
| Shredder | Paper Mfg. | M7 | 400% |
| Slicer | Plastics Mfg | M7 | 600% |
| Stamping Die | Steel Furniture | D2 | 1000% |
| Tap | Tool Maker | C2 Carbide | 600% |
| Wood cutting | Pro Woodworker | HSS | 500% |
| Corrosion | University Study | S2,M2,4142,316 | Reduced all Corrosion |